To ensure consistent results, JIS K 6251 specifies rigorous testing conditions: JIS K 6251:2004 Rubber, vulcanized or thermoplastic
Samples must be conditioned at and 50 ± 5% relative humidity for at least 3 hours before testing.
: The percentage increase in length that occurs before the rubber specimen snaps.